Store Hours:
7:30am - 5:00pm M-F
8:00am - 12:00pm Saturday
Cincinnati
(513) 489-9111
6130 Cornell Rd
Cincinnati, OH 45242
Norwood
(513)651-9111
4686 Paddock Rd
Cincinnati, OH 45229
Columbus
(614)224-9111
831 Harmon Ave
Columbus, OH 43223
Erlanger
(859)341-9111
2930 Crescent Springs Rd
Erlanger, KY 41018
Lexington
(859)254-9111
970 West New Circle Rd
Lexington, KY 40511
Dayton
(937)866-9111
801 E 1st St
Dayton, OH 45402
PRODUCTS
MANUFACTURERS
BACK TO JANELL.COM
BROWSE CATEGORIES
> Bolt
> Nail
> Nut
> Screws
> Staple
> Washer
Abrasives
Adhesives | Sealants | Tape
Concrete and Asphalt Chemicals
Concrete and Asphalt Products
Concrete Forming
Construction Fabrics
Decorative Concrete
Drill Bits and Drilling Accessories
Equipment
Erosion Control | SWPPP
Fasteners | Anchors
Fastening Pins & Inserts
Hand Tools
Hardscapes
Industrial Pumps
Leveling | Measuring | Surveying
Lumber Products
Masonry
Material Handling | Storage | Containment
Outdoor Products
Power Tool Accessories
Power Tools
Presses & Shop Equipment
Rebar and Wire Mesh
Safety Equipment and Products
Shop Vacuums
Structural Hardware
Tiles and Detectable Warning Pads
Tilt Up
Tool Storage | Job Site Boxes | Truck Boxes | Transfer Tanks
Trench Drains
Waterproofing Products
Home
/
Categories
/
Power Tools
/
Grinders, Polishers & Sanders
/
Finishing Tools
/
Jointers
/
Search:
Sponge Rubber EXP Expansion Joint
Sponge Rubber EXP Expansion Joint
Right Pointe
Sponge Rubber Expansion Joint is composed of economical re-bonded sponge rubber particles manufactured to a consistent density and size. This very workable material has a recovery rate of 95% or more of the original thickness and a density exceeding 30 pounds/cu. ft.
(click image to enlarge)
Quick Overview
Features and Benefits:
Designed for high performance, low tolerance criteria projects
Excellent recovery properties for installations with wide temperature variations
For isolation applications or between materials with dissimilar coefficients of expansion
Meets or exceeds all specifications.
Resilient - recovers 95% of original thickness after compression.
Resists water infiltration.
Easy to handle and install
Petroleum resistant
Use And Applications:
Sponge Rubber Expansion Joint is suitable for use with a wide variety of concrete construction projects. Noted for its excellent recovery properties, it is frequently used in applications that experience rapid changes in temperature.
Click here for the MSDS
Interested in this item or want more information?
Call Mon. - Fri. 7:30 AM - 5:00 PM / Sat. 8:00 PM - 12:00 PM
Phone: (888) 489-9111
Email:
info@janell.com
Can't find what you want? Give us a call and we can help you find it.
Details
Size Information:
Thickness: 1/4", 3/8", 1/2", 3/4", 1"
Standard Lengths: 54"
Slab Width: 36"
Cut to Size: 2" to 36" in 1/2" increments
Typical Properties:
Compression (to 50% of original)
50-500psi
Water Absorption by Weight
Average of closed and open-celled sponge Compression Set 10% maximum. ASTM Method: ½" samples compressed for 22 hours @ 70°F - 24 hour recovery
Density
30 PCF minimum
Temperature Resistance Low
-40°F
Temperature Resistance High Continuous
+180°F
Temperature Resistance High Intermittent
+220°F
Accelerated Aging:
Good
ASTM Method:
7 days at 158°F-lineal shrinkage maximum 2%) Flexibility 180° bend without cracking
Tensile Strength (minimum)
25psi
Elongation (minimum)
75%
Additional Information
Manufacturer: Right Pointe